性能项目 | 试验条件[状态] | 测试方法 | 测试数据 | |
比重 | ASTMD792 | 1.30 | g/cm3 | |
吸水率 | 23°C,24hr | ASTMD570 | 0.50 | % |
吸水率 | 饱和,23°C | ASTMD570 | 0.50 | % |
洛氏硬度(M级) | ASTMD785 | 99 | ||
拉伸模量-1%正割(23°C) | ASTMD638 | 4480 | MPa | |
抗张强度(屈服,23°C) | ASTMD638 | 110 | MPa | |
伸长率 | 屈服,23°C | ASTMD638 | 4.9 | % |
伸长率 | 断裂,23°C | ASTMD638 | 40 | % |
弯曲模量(23°C) | ASTMD790 | 4140 | MPa | |
弯曲强度(23°C) | ASTMD790 | 179 | MPa | |
压缩强度(23°C) | ASTMD695 | 118 | MPa | |
剪切强度(23°C) | ASTMD3846 | 52.4 | MPa | |
摩擦系数1 | 0.18 | |||
悬壁梁缺口冲击强度(23°C) | ASTMD256 | 51 | J/m | |
载荷下热变形温度(1.8MPa,未退火,6.35mm) | ASTMD648 | 160 | °C | |
连续使用温度 | 260 | °C | ||
熔融温度 | 334 | °C | ||
线形热膨胀系数-流动 | ASTMD696 | 4.7E-5 | cm/cm/°C | |
导热系数 | ASTMC177 | 0.25 | W/m/K | |
表面电阻率 | ASTMD257 | 1.0E+16 | ohms | |
体积电阻率(23°C) | ASTMD257 | 4.9E+16 | ohmscm | |
介电强度 | ASTMD149 | 7.5 | kV/mm | |
UL阻燃等级 | UL94 | V-0 | ||
LimitingPressureVelocity-1200in/min(20°C) | 170000 | psifpm |
PEEK塑料供应商,长期销售德国恩欣格生产的PEEK原料,以上是“PEEK TECAPEEK® TECAPEEK®”塑胶料的物性表参数.近期代理商可转仓交易:日本瑞翁 丙烯酸 HyTemp® 4053EP
美国Ecomass PA共聚物 Ecomass® 1005ZD96 填料,Ecomass,美国Ecomass.
德国巴斯夫 TPU Konz 704 注塑
利安德巴塞尔 HDPE 4261 AG UV 良好的耐化学性,高级开裂,抗应力裂纹,高耐冲击,中等耐热性 吹塑应用,工业应用,罐
美国RTP PEEK 2282 TFE 15 经润滑
英国Techsil Rubber Techsil® RTV2420
朗盛(拜耳) PA6 BKV35HTS 35%玻纤增强,较H1,0和H2,0有更好的热稳定性,连续工作温度可高达160℃
韩国可隆 PA66 KOPA® KN333HB440BL 尺寸稳定性良好
意大利科因 TPU 8020 良好的撕裂强度,耐化学性良好,耐磨蚀性良好,耐气候影响性能良好,韧性良好
日本宇部 LDPE C480 其它 交联用树脂,电缆料
意大利兰蒂奇 PA66 A RV300AE 玻璃纤维增强材料,30%填料按重量,高刚性,阻燃性能
沙伯基础 PPA LNP™ LUBRICOMP™ UFL36S compound
加拿大ACLO ABS ACCUCOMP™ ABS811L 中等抗撞击性
法国Eurostar PA66 Star L PA66 D91 填料,芳族聚酰胺纤维.
美国RTP PP 154 阻燃性能
● PEEK 沙伯基础 LNP LUBRICOMP LL002 compound
耐磨损性良好,润滑,注射成型
● PEEK 美国RTP RTP 2299 X 108578 A
填料:长玻璃纤维, 30% 填料按重量。
● PEEK 沙伯基础 LNP STAT-KON LX04420C compound
● PEEK 美国RTP 2207 HF UP
高流动,注塑
● PEEK 德国赢创(德固赛) VESTAKEEP 4000FP